Podcast Episode 10
Solving Metal Casting Defects is a tricky process and there is no Black and White.
However Mr Dhumane comes pretty close with his Root cause Analysis Framework for Casting Defect Identification.
During his Long Career, He has Worked as Plant Manager for Large Foundries like KSB Pumps, Kirloskar Ferrous, Ashok Iron and Gwasf and Powal Auto.
Mr Sharad Dhumane is now settled in Pune, MH India as a Foundry Freelancer for his Firm Metals and Creations.
Today, We sit down with SharadJi to Grab some of his Secrets on Record.
You can Reach Him here :
Linkedin : https://www.linkedin.com/in/sharad-dhumane-4ba809101/
The Host of the Show is Ian Nazareth who has 10 Years of Experience in the Foundry Industry.
The Foundry Podcast is a Channel where we discuss all things Foundry Related in One Place.From having Industry Veterans on our Show to the Latest News and the Most Advanced Tech Innovations in the Market Today.If You're in the Foundry Industry, You've come to the Right Place!
You can Connect with Ian here :
Linkedin : https://www.linkedin.com/in/ian-nazareth-095b14ab/
Email : marketing@metally.co.in
Enjoy!
0:00 Teaser.
0:37 Intro.
2:50 Sharad's Background.
3:20 KSB Pumps.
4:35 Ashok Iron Works Belgaum.
6:30 Porwal Auto.
7:32 Gwasf Foundry.
8:46 Kirloskar Ferrous.
9:32 What is a Casting Defect?
11:02 Why do Casting Defects Occur?
13:20 Benchmarks Rejection Rates per Grade.
15:11 How to Reduce Rejection Rate?
16:39 Most Commom Casting Defect Seen.
20:23 Sharad's Secret Tool.
21:20 Two Types of Slag.
25:14 Reading Material for Foundries.
27:34 6 Sigma Tools.
30:00 Sharad's 1300 Member Whatsapp Group.
34:22 Experiences from All around India.
36:05 What Sharad Does Today - Metals and Creations.
36:43 Working with Dana Corporation America.
37:48 Sharad and Forging.
40:33 Sharad's View on Foundry Podcast.
43:20 Yogayata Vikas Trainer - IIF.
46:29 Next Topic with Sharad.
48:00 Outro.